The objective of this study was to evaluate the interfacial fracture toughness (IFT) of composite cement with dispersed filler (DF) versus polymer-infiltrated ceramic network (PICN) computer-aided design and computer-aided manufacturing (CAD-CAM) composite blocks after 2 different surface pretreatments using the notchless triangular prism (NTP) test. Two DFs (Cerasmart [CRT] and Lava Ultimate [LVA]), 2 PICNs (Enamic [ENA] and experimental PICN [EXP]), and e.max CAD lithium disilicate glass-ceramic (EMX, control) prism samples were bonded to their counterparts with Variolink Esthetic DC composite cement after either hydrofluoric acid etching (HF) or gritblasting (GR). Both procedures were followed by silanization. All samples ( n = 30 per group) were thermocycled (10,000 cycles) and tested for their IFT in a water bath at 36°C. Moreover, representative samples from each group were subjected to a developed interfacial area ratio (Sdr) measurement by profilometry and scanning electron microscopy (SEM) characterization. EXP-HF gave the highest IFT (1.85 ± 0.39 MPa·m1/2 ), followed by EMX-HF and ENA-HF, while CRT-HF gave the lowest (0.15 ± 0.22 MPa·m1/2 ). PICNs gave significantly better results with HF, and DF showed better results with GR. A 2-way analysis of variance indicated that there were significantly higher IFT and Sdr for PICNs than for DF. A positive correlation ( r² = 0.872) was found between IFT and Sdr. SEM characterization showed the specific microstructure of the surface of etched PICNs, indicating the presence of a retentive polymer-based honeycomb structure. Etching of the typical double-network microstructure of PICNs causes an important increase in the Sdr and IFT, while DF should be gritblasted. DF exhibited significantly lower Sdr and IFT values than PICNs. The present results show the important influence of the material class and surface texture, and consequently the micromechanical bond, on the adhesive interface performance of CAD-CAM composites.
Full text links
Related Resources
Trending Papers
Consensus Statement on Vitamin D Status Assessment and Supplementation: Whys, Whens, and Hows.Endocrine Reviews 2024 April 28
The Tricuspid Valve: A Review of Pathology, Imaging, and Current Treatment Options: A Scientific Statement From the American Heart Association.Circulation 2024 April 26
British Society of Gastroenterology guidelines for the management of hepatocellular carcinoma in adults.Gut 2024 April 17
Interstitial Lung Disease: A Review.JAMA 2024 April 23
Ventilator Waveforms May Give Clues to Expiratory Muscle Activity.American Journal of Respiratory and Critical Care Medicine 2024 April 25
Systemic lupus erythematosus.Lancet 2024 April 18
Acute Kidney Injury and Electrolyte Imbalances Caused by Dapagliflozin Short-Term Use.Pharmaceuticals 2024 March 27
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app