Effect of a silane and phosphate functional monomer on shear bond strength of a resin-based luting agent to lithium disilicate ceramic and quartz materials.
Journal of Oral Science 2018 September 24
This study examined the effect of silane and phosphate functional monomer on bond strengths between a resin-based luting agent joined to a lithium disilicate ceramic (IPS e.max) and silica (quartz) materials. The e.max and quartz specimens were assigned to 6 groups with different priming/bonding agents, namely, Clearfil Porcelain Bond Activator, Clearfil Photo Bond, Clearfil Photo Bond Universal with Clearfil Porcelain Bond Activator, Clearfil Photo Bond Catalyst with Clearfil Porcelain Bond Activator, Clearfil Photo Bond with Clearfil Porcelain Bond Activator, and unprimed. The corresponding specimens were bonded by using a resin-based luting agent (Panavia V5). Shear bond strengths were determined before and after 5,000 thermocycles. For both the e.max and quartz specimens, the Clearfil Photo Bond Universal with Clearfil Porcelain Bond Activator group had the highest pre- and post-thermocycling bond strength values. Combined use of silane in the acidic environment of a phosphate functional monomer and initiators enhances bond strength of a resin-based luting agent to e.max ceramic and quartz materials.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app