A Simple Synthesis and Microstructure Analysis of Human Peptide LL-37@Gold Nanoparticles (Known as LL-37@AuNPs) Conjugates as Antimicrobials and Substances for Wound Healing.

Materials 2023 December 17
The basis of the present study is a straightforward method involving fewer chemical species for conjugating gold nanoparticles (AuNPs) with the antimicrobial peptide LL-37 designated as LL-37@AuNPs. Investigating the microstructure characteristics of the resulting materials and their potential as antibacterial and wound-healing substances are the main objectives of this study. Zeta (ζ) potential, Fourier transform infrared (FTIR), X-ray diffraction (XRD), field effect scanning electron microscopy (FE-SEM), energy dispersive X-ray diffraction (EDS), transmission electron microscopy (TEM), and UV-Vis spectrophotometry were used to analyze the physico-chemical properties of LL-37@AuNPs. The magnitude of LL-37's zeta potential and the LL-37@AuNPs show that the specimens are electrically stable and resistant to flocculation and coagulation. The surface plasmon resonance (RPS) of AuNPs, which is positioned at a wavelength of about 531 nm, was found to be unaffected by the presence of the LL-37 antimicrobial peptide. The FTIR data show the functional group characteristics of the LL-37@AuNPs vibration bands, and the XRD diffractogram confirms the formation of the LL-37@AuNPs conjugate nanocomposite. Based on FE-SEM and TEM data, the bulk of AuNPs were found to have a circular shape, with an average size of about 22.88 ± 8.21 nm. It was discovered that the LL-37@AuNPs had a good ability to inhibit S. aureus from growing. The wound-healing percentage reached 85% on day 12 of the trial, significantly greater than the results of the negative controls. LL-37@AuNPs(4) is the sample that had the highest percentage of wound healing between days 3 and 12. Moreover, sample LL-37@AuNPs(4) contains 0.45 µL of LL-37, whereas sample LL-37@AuNPs(2) contains 0.22 µL of LL-37. The faster wound-healing rate in LL-37@AuNPs(4) was believed to be due to a higher concentration of LL-37, which was able to stop S. aureus from developing while suppressing the inflammation surrounding the wound. The study's findings reveal that LL-37@AuNPs might be made using a straightforward process, making them a powerful antibacterial and therapeutic substance. However, before this discovery is applied in the field of medicine, a more thorough investigation is necessary.

Full text links

We have located links that may give you full text access.
Can't access the paper?
Try logging in through your university/institutional subscription. For a smoother one-click institutional access experience, please use our mobile app.

Related Resources

For the best experience, use the Read mobile app

Mobile app image

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app

All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.

By using this service, you agree to our terms of use and privacy policy.

Your Privacy Choices Toggle icon

You can now claim free CME credits for this literature searchClaim now

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app