Uniform coating of Ta 2 O 5 on vertically aligned substrate: A prelude to forced flow atomic layer deposition.
Review of Scientific Instruments 2017 June
Uniform tantalum oxide thin films, with a growth rate of 0.6 Å/cycle, were fabricated on vertically aligned, 10 cm-long, silicon substrates using an innovative atomic layer deposition (ALD) design. The ALD system, with a reaction chamber depth of 13.3 cm and 18 vertical enclosed channels (inner diameter 1.3 cm), was coupled with a shower-head type precursor conduit plate bearing 6 radial channels. This design enabled deposition on 6 silicon substrates at a time. The degrees of non-uniformity of deposits along the length of the silicon wafer and across different positions in the ALD chamber were found to be 1.77%-6.21% and 3.27%-5.45%, respectively. A further advantage of the design is that the conduit plate may be modified and the number of channels increased to process 18 substrates simultaneously, thus moving toward efficient and expedited ALD systems.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app