Chromium and cobalt in leather: A Danish market survey.
Contact Dermatitis 2024 July 28
INTRODUCTION: Leather has been a significant source of chromium (Cr) allergy in Denmark since the 1990s. More recently, cobalt (Co) allergy has been identified in leather as a source of allergic contact dermatitis.
OBJECTIVES: To measure Cr and Co levels in Danish leather goods.
METHODS: A total of 87 leather samples were collected, all tanned in Europe. Handheld X-ray fluorescence (XRF) device was used to screen for the presence of Cr and Co. The 20 leather samples with the highest concentrations of Co and Co were tested using International Organization for Standardization (ISO)-standards.
RESULTS: XRF analysis showed Cr in 78/87 (83.9%) samples and Co in 52/87 (59.7%), with average concentrations of 41 mg/kg (range: 0.0-77 mg/kg) and 0.22 mg/kg (range: 0.0-2.9 mg/kg), respectively. ISO 10195 and 17 075-1 testing identified Cr (VI) in 7 out of 20 samples (1.4; 0.3-4.2 mg/kg), while ISO 17072-1 detected Co in 6 of 20 samples, averaging 3.95 mg/kg (range: 0.22-7.9 mg/kg).
CONCLUSION: Most leather samples contained Cr, which was expected, while Cr (VI) was detectable in seven out of twenty tested samples but only detected in one product above the regulatory limit of 3 mg/kg. A potentially significant concentration was found for Co.
OBJECTIVES: To measure Cr and Co levels in Danish leather goods.
METHODS: A total of 87 leather samples were collected, all tanned in Europe. Handheld X-ray fluorescence (XRF) device was used to screen for the presence of Cr and Co. The 20 leather samples with the highest concentrations of Co and Co were tested using International Organization for Standardization (ISO)-standards.
RESULTS: XRF analysis showed Cr in 78/87 (83.9%) samples and Co in 52/87 (59.7%), with average concentrations of 41 mg/kg (range: 0.0-77 mg/kg) and 0.22 mg/kg (range: 0.0-2.9 mg/kg), respectively. ISO 10195 and 17 075-1 testing identified Cr (VI) in 7 out of 20 samples (1.4; 0.3-4.2 mg/kg), while ISO 17072-1 detected Co in 6 of 20 samples, averaging 3.95 mg/kg (range: 0.22-7.9 mg/kg).
CONCLUSION: Most leather samples contained Cr, which was expected, while Cr (VI) was detectable in seven out of twenty tested samples but only detected in one product above the regulatory limit of 3 mg/kg. A potentially significant concentration was found for Co.
Full text links
Related Resources
Trending Papers
Prevention and management of venous thrombosis in patients with cirrhosis.British Journal of Haematology 2024 August 26
Antibodies in Autoimmune Neuropathies: What to Test, How to Test, Why to Test.Neurology 2024 August 27
Arrhythmogenic Mitral Valve Prolapse: Can We Risk Stratify and Prevent Sudden Cardiac Death?Arrhythmia & Electrophysiology Review 2024
Heart-Lungs interactions: the basics and clinical implications.Annals of Intensive Care 2024 August 12
An Updated Review of the Management of Chronic Heart Failure in Patients with Chronic Kidney Disease.Reviews in Cardiovascular Medicine 2024 April
Myocardial ischaemic syndromes: a new nomenclature to harmonize evolving international clinical practice guidelines.European Heart Journal 2024 August 30
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app