TiO 2 Nanomembranes Fabricated by Atomic Layer Deposition for Supercapacitor Electrode with Enhanced Capacitance.
Nanoscale Research Letters 2019 March 14
TiO2 is a promising environment friendly, low cost, and high electrochemical performance material. However, impediments like high internal ion resistance and low electrical conductivity restrict its applications as electrode for supercapacitor. In the present work, atomic layer deposition was used to fabricate TiO2 nanomembranes (NMs) with accurately controlled thicknesses. The TiO2 NMs were then used as electrodes for high-performance pseudocapacitors. Experimental results demonstrated that the TiO2 NM with 100 ALD cycles had the highest capacitance of 2332 F/g at 1 A/g with energy density of 81 Wh/kg. The enhanced performance was ascribed to the large surface area and the interconnectivity in the case of ultra-thin and flexible NMs. Increased ALD cycles led to stiffer NMs and decreased capacitance. Moreover, one series of two supercapacitors can light up one light-emitting diode with a working voltage of ~ 1.5 V, sufficiently describing its application values.
Full text links
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app