Effect of Surface Roughness on Pitting Corrosion of 2205 Duplex Stainless Steel Investigated by Electrochemical Noise Measurements.
Materials 2019 March 5
The influence of surface roughness on the pitting corrosion behaviour of 2205 duplex stainless steel (DSS) in a chloride-containing environment was investigated using electrochemical noise (EN) techniques and morphology observation. A rougher surface condition increased the frequency of pit initiation because of the increase in more occluded pit sites. Rough surface finish also accelerated pit growth by increasing the actual dissolution rate in the pit. Metastable pits on rougher surfaces had longer lifetimes and grew to larger sizes, as their inner chemical environment was more easily maintained. However back-scatter images showed that pitting initiates on DSS 2205 regardless of the roughness condition.
Full text links
Trending Papers
A Personalized Approach to the Management of Congestion in Acute Heart Failure.Heart International 2023
Potential Mechanisms of the Protective Effects of the Cardiometabolic Drugs Type-2 Sodium-Glucose Transporter Inhibitors and Glucagon-like Peptide-1 Receptor Agonists in Heart Failure.International Journal of Molecular Sciences 2024 Februrary 21
The Effect of Albumin Administration in Critically Ill Patients: A Retrospective Single-Center Analysis.Critical Care Medicine 2024 Februrary 8
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app