Bonding strengths to porcelain: An in vitro study of ultrasonic and conventional tooth preparation and etching.
Journal of Conservative Dentistry : JCD 2019 January
Objective: To compare the bond strength of porcelain to enamel and dentin preparations finished with either ultrasonic instruments or diamond burs, with or without acid etching.
Materials and Methods: A total of 140 extracted bovine incisor teeth were divided into two groups, enamel and dentin. A split tooth model was employed: each tooth having a randomly allocated combination of diamond burs, ultrasonic instrument, etching, and no etching treatments on their labial surface. Lithium disilicate glass ceramic specimens were bonded to the prepared surfaces and tensile testing was carried out. Force was applied to failure, and linear mixed models were used to analyze the data.
Results: Etching increased the bond strength of the dentin samples by 7.63 MPa ( P < 0.001). When bonding to dentin, ultrasonic instrument preparation produced a 2.88 MPa greater bond strength compared to burs ( P < 0.001).
Conclusion: Ultrasonic preparation produced greater bond strengths compared to rotary instruments. Etching improved the bond strength of all preparations, with enamel having consistently greater bonding values than dentin.
Materials and Methods: A total of 140 extracted bovine incisor teeth were divided into two groups, enamel and dentin. A split tooth model was employed: each tooth having a randomly allocated combination of diamond burs, ultrasonic instrument, etching, and no etching treatments on their labial surface. Lithium disilicate glass ceramic specimens were bonded to the prepared surfaces and tensile testing was carried out. Force was applied to failure, and linear mixed models were used to analyze the data.
Results: Etching increased the bond strength of the dentin samples by 7.63 MPa ( P < 0.001). When bonding to dentin, ultrasonic instrument preparation produced a 2.88 MPa greater bond strength compared to burs ( P < 0.001).
Conclusion: Ultrasonic preparation produced greater bond strengths compared to rotary instruments. Etching improved the bond strength of all preparations, with enamel having consistently greater bonding values than dentin.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app