Immobilisation of high-arsenic-containing tailings by using metallurgical slag-cementing materials.

Chemosphere 2019 Februrary 9
The mixture of finely ground blast furnace slag (BFS), basic oxygen furnace (BOF) steel slag (SS), and flue gas desulfurisation (FGD) gypsum could be used as cement to solidify heavy metals. In this study, these cementitious materials were combined with high-arsenic-containing tailings to form cemented backfill material (CBM). The results indicated that the optimal design of CBM was that of specimen CBM2 which showed good early strength (10.09 MPa) at a curing age of 3 days containing 60% BF slag, 30% SS, and 10% gypsum. And the arsenic leaching concentration of CBM2 at a curing age of 7 days and 28 days were both less than the limits specified in standards for drinking water quality (Chinese Standard GB 5749-2006). The predominant hydration products of CBM2 contained rod-like ettringite and amorphous C-S-H gel both of which promote arsenic solidification.

Full text links

We have located links that may give you full text access.
Can't access the paper?
Try logging in through your university/institutional subscription. For a smoother one-click institutional access experience, please use our mobile app.

Related Resources

For the best experience, use the Read mobile app

Mobile app image

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app

All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.

By using this service, you agree to our terms of use and privacy policy.

Your Privacy Choices Toggle icon

You can now claim free CME credits for this literature searchClaim now

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app