Removal of cyanide adsorbed on pyrite by H 2 O 2 oxidation under alkaline conditions.

Large amounts of cyanide tailings are produced during the cyanidation process in gold extraction, which are hazardous solid wastes due to the toxic cyanide. Pyrite is one of the main minerals in cyanide tailings. The removal of cyanide adsorbed on pyrite by H2 O2 oxidation under alkaline conditions was investigated in this study. It was found that the removal efficiency was positively correlated with pH from 5 to 12, but remained almost constant when pH was higher than 12. The highest cyanide removal efficiency of 91.10% was achieved by adding no less than 0.6 wt.% of H2 O2 . Cyanide removal was positively correlated with the CN- adsorption amount between 1.06 and 8.5 mg/g, and temperature between 25 and 85°C. The removal of cyanide adsorbed on pyrite by H2 O2 oxidation under alkaline conditions was due to the oxidation of pyrite. Hexacyanoferrate, thiocyanate and sulfate were generated with mole ratios of about 2.03:1.12:3.17 during the cyanide removal.

Full text links

We have located links that may give you full text access.
Can't access the paper?
Try logging in through your university/institutional subscription. For a smoother one-click institutional access experience, please use our mobile app.

Related Resources

For the best experience, use the Read mobile app

Mobile app image

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app

All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.

By using this service, you agree to our terms of use and privacy policy.

Your Privacy Choices Toggle icon

You can now claim free CME credits for this literature searchClaim now

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app