A new membrane electro-deposition based process for tin recovery from waste printed circuit boards.
Journal of Hazardous Materials 2016 March 6
The current research investigated a process combining leaching, purification and membrane electrodeposition to recover tin from the metal components of WPCBs. Experimental results showed that with a solid liquid ratio of 1:4, applying 1.1 times of stoichiometric SnCl4 dosage and HCl concentration of 3.5-4.0 mol/L at a temperature of 60-90°C, 99% of tin can be leached from the metal components of WPCBs. The suitable purification conditions were obtained in the temperature range of 30-45°C with the addition of 1.3-1.4 times of the stoichiometric quantity of tin metal and stirring for a period of 1-2h; followed by adding 1.3 times of the stoichiometric quantity of Na2S for sulfide precipitation about 20-30 min at room temperature. The purified solution was subjected to membrane electrowinning for tin electrodeposition. Under the condition of catholyte Sn(2+) 60 g/L, HCl 3 mol/L and NaCl 20 g/L, current density 200 A/m(2) and temperature 35°C, a compact and smooth cathode tin layer can be obtained. The obtained cathode tin purity exceeded 99% and the electric consumption was less than 1200 kW h/t. The resultant SnCl4 solution generated in anode compartment can be reused as leaching agent for leaching tin again.
Full text links
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app