In situ crystal growth of zeolitic imidazolate frameworks (ZIF) on electrospun polyurethane nanofibers.
This paper reports for the first time in situ crystal growth of ZIF-8 on electrospun polyurethane (PU) nanofibers. In SEM images, continuous and compact ZIF-8 nanocrystals grow along electrospun PU nanofibers. The highest loading capacity of ZIF-8 on PU reaches 63%. By N2 adsorption-desorption, ZIF-8-PU shows a high surface area of 566 cm(2) g(-1). Combining the good flexibility of PU with the high adsorption properties of ZIF-8, ZIF-8-PU can be easily tailored into clothes or other forms as adsorption material. Furthermore, the gas adsorption ability of ZIF-8-PU was measured for H2, N2, O2 and CO2 at room temperature (20 °C) under different pressure gradients. The results show that the adsorption capacity of ZIF-8-PU for CO2 is nearly 11 times that for H2, 50 times that for O2 and 75 times that for N2 at 800 mmHg.
Full text links
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app