Diffusion bonding of mismatch dental alloys.

The diffusion bonding of Ti-6Al-4V and Co-Cr-Mo dental alloys has been investigated in terms of the atoms diffusion, the microstructure evolution, and the bonding strength. The bonding performance reveals asymmetry diffusion profiles for both the Co and Cr in Ti-6Al-4V and the Ti in Co-Cr-Mo alloy. Their diffusion coefficients (Arrhenius relations) have been established based on the experiments. Co and Cr diffusion into Ti-6Al-4V leads to alpha --> beta transformation and the intermetallics-formation. Maximum bonding strength occurs at about 840 degrees C. The bonding joint fails under the shear stress in the Ti-6Al-4V side near the bonding interface in brittle manner. The intermetallics in the diffusion layer together with the unbonded areas and other flaws in the bonding interface are responsible for the shear brittle fracture, which also weaken the bonding strength.

Full text links

We have located links that may give you full text access.
Can't access the paper?
Try logging in through your university/institutional subscription. For a smoother one-click institutional access experience, please use our mobile app.

For the best experience, use the Read mobile app

Mobile app image

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app

All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.

By using this service, you agree to our terms of use and privacy policy.

Your Privacy Choices Toggle icon

You can now claim free CME credits for this literature searchClaim now

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app