Daishi Nakase, Kei Kubochi, Jin Kitani, Junichi Honda, Taro Iwasaki, Futoshi Komine
The aim of the present study was to evaluate the influence of two different internal surface treatments, namely, the firing of feldspathic porcelain before or after zirconia sintering, on the marginal and internal adaptation of laminate veneers (LVs) made of high-translucent zirconia. A total of 33 zirconia LVs were fabricated using a CAD/CAM system and divided into three groups based on the internal surface treatment method: the pre-firing (PRE) group involved firing feldspathic porcelain before zirconia sintering, the post-firing (POS) group involved firing feldspathic porcelain after zirconia sintering, and the no treatment (NT) group involved no application of feldspathic porcelain...
October 24, 2023: Journal of the Mechanical Behavior of Biomedical Materials